当前位置: 首页 > 文章 > 辙叉用耐磨钢回火试验 农业科技与装备 2019 (2) 42-43+46
Position: Home > Articles > Tempering Test of Wear-resisting Steel for Frog Agricultural Science & Technology and Equipment 2019 (2) 42-43+46

辙叉用耐磨钢回火试验

作  者:
张振忠;刘文闯;王振伟
单  位:
中铁山桥集团有限公司;燕山大学
关键词:
有轨电车;辙叉;耐磨钢;钢轨;回火
摘  要:
采用对比试验的方法,从200℃开始设置6种不同温度,研究耐磨钢的焊后合理回火温度。结果表明,综合耐磨钢在微观金相组织、表面硬度、拉伸性能、冲击性能方面的变化情况,焊后回火温度以350℃为宜。
译  名:
Tempering Test of Wear-resisting Steel for Frog
作  者:
ZHANG Zhenzhong;LIU Wenchuang;WANG Zhenwei;China Railway Shanhaiguan Bridge Group Co., Ltd;Yanshan University;
单  位:
ZHANG Zhenzhong%LIU Wenchuang%WANG Zhenwei%China Railway Shanhaiguan Bridge Group Co., Ltd%Yanshan University
关键词:
tramcar;;frog;;wear-resisting steel;;rail;;tempering
摘  要:
Adopting the method of contrast test, 6 different temperature was set from 200 ℃ to study the wear-resisting steel after welding tempering temperature. The results showed that the composite wear-resisting steel changes in the aspects of microscopic metallographic organization, surface hardness, tensile properties, impact performance, and it is advisable to tempering temperature 350℃ after welding.